The development of metal 3D printing has become increasingly sophisticated over time. At the same time, metal 3D printing has become a crucial part of Baosheng Industry’s business. This article, from Baosheng’s perspective, aims to share how we tell the story that each of our clients wishes to have told, using the 5 well-known metal 3D printing techniques that we are familiar with.
Metal additive manufacturing currently operates on two primary material forms: powder bed fusion and wire-fed deposition. While emerging technologies like Liquid Metal Jetting (LMJ) show potential, they fundamentally remain derivatives of powder-binding systems. Industrial-grade metal 3D printers continue to present significant capital investment requirements and specialized operational expertise.
This article provides a technical breakdown of five mainstream metal 3D printing processes and their compatible material systems, analyzing their intrinsic value in industrial applications.
1.Selective Laser Sintering (SLS)
Selective Laser Sintering (SLS), as a representative powder bed fusion technology, is fundamentally based on a non-equilibrium liquid-phase sintering mechanism. Under laser energy density (50-100 J/mm³), the surface layer of powder particles undergoes partial melting to form liquid-phase envelopes, while the core retains a solid crystalline structure. During this process, melt-driven capillary forces induce solid particle rearrangement (displacement ≈15-40 μm), followed by liquid-phase solidification to form neck connections, achieving green part densities of 60-85% theoretical.
System Architecture and Kinetic Characteristics
The SLS system comprises a powder supply cylinder, build cylinder, and closed-loop thermal control modules (protective atmosphere purity ≥99.995% N₂/Ar). The process cycle includes:
- Powder piston quantized elevation (layer thickness accuracy ±10 μm) with a roller spreading 50-100 μm layers at 0.8-1.2 m/s;
- 1070 nm fiber laser selectively scans sliced paths (scan speed 2-4 m/s, spot diameter 70-150 μm), inducing semi-solid phase transitions;
- Build piston incrementally descends for layer-wise stacking (typical layer thickness 20-100 μm).
| Process Step | Details |
|---|---|
| Powder Piston Elevation | Quantized elevation with layer thickness accuracy of ±10 μm |
| Powder Spreading | Roller spreads 50-100 μm layers at 0.8-1.2 m/s |
| Laser Scanning | 1070 nm fiber laser scans sliced paths (2-4 m/s, spot diameter 70-150 μm) |
| Build Piston Descending | Incremental descent for layer-wise stacking (20-100 μm per layer) |
2. SLS Process Limitations and Defects
Despite partial melting reducing thermal stress accumulation (residual stress <150 MPa), solid-liquid coexistence introduces three critical defects:
- Porosity (15-30%): Unmelted particles hinder densification, creating grain boundary micropores (pore size 5-20 μm);
- Balling Effect (contact angle >130°): High-viscosity melt (η≈10³-10⁴ Pa·s) causes melt pool fragmentation, forming spherical satellites (diameter 30-100 μm), resulting in surface roughness Ra of 10-25 μm;
- Anisotropic Mechanical Properties: Tensile strength along the build direction is 20-40% lower than in X/Y axes (e.g., 316L stainless steel: Z-axis ≈450 MPa vs. X/Y-axis ≈580 MPa).
| Defect | Cause | Impact | Typical Size |
|---|---|---|---|
| Porosity | Unmelted particles impede densification, creating micropores | Grain boundary micropores | 5-20 μm |
| Balling Effect | High-viscosity melt fragments into spherical satellites | Increases surface roughness, poor quality | 30-100 μm (diameter) |
| Anisotropic Mechanical Properties | Solid-liquid coexistence results in directional mechanical strength differences | Lower tensile strength along build direction | Z-axis ≈ 450 MPa, X/Y-axis ≈ 580 MPa |
3. Process Optimization Strategies
- Powder Engineering: Plasma-spheroidized powders (sphericity >0.92) with nano-SiO₂ coatings (thickness 50-100 nm) reduce melt viscosity by 18-25%;
- Energy Field Modulation: Dual-laser interference (phase difference π/2) induces melt pool oscillations, breaking oxide films and reducing balling rate to <5%;
- Post-Processing: Hot isostatic pressing (HIP, 1200°C/100 MPa/4h) increases density to >99.2%, complying with ASTM F3301.
| Strategy | Description | Effect |
|---|---|---|
| Powder Engineering | Plasma-spheroidized powders with nano-SiO₂ coatings | Reduces melt viscosity by 18-25% |
| Energy Field Modulation | Dual-laser interference (phase difference π/2) | Breaks oxide films, reduces balling rate to <5% |
| Post-Processing | Hot isostatic pressing (HIP, 1200°C/100 MPa/4h) | Increases density to >99.2% |
4.SLS System Specifications
| Component | Specification |
|---|---|
| Powder Cylinder | Contains feed powder, controlled by piston for accurate elevation |
| Build Cylinder | Used for layer-wise stacking with incremental piston descent |
| Thermal Control Modules | Closed-loop, protective atmosphere purity ≥99.995% N₂/Ar |
| Laser Specifications | 1070 nm fiber laser, scan speed 2-4 m/s, spot diameter 70-150 μm |

2. Selective Laser Melting (SLM)
Selective Laser Melting (SLM), an advanced derivative of SLS technology, distinguishes itself through full-melting metallurgical mechanisms and submicron-scale energy field control. Utilizing ytterbium-doped fiber lasers (1070 nm wavelength) with power densities of 10⁶-10⁷ W/cm², SLM completely melts 20-50 μm metal powders, achieving over 99.5% density via Marangoni convection-driven melt pool dynamics (depth ≈100-300 μm).
SLM Process Dynamics and System Architecture
- Energy Field Modulation:
- Adjustable laser power (200-1000 W), focused spot diameter (30-80 μm), and scan speed (1-15 m/s) via galvanometer systems;
- Bidirectional staggered scanning (67° hatching angle) reduces anisotropy to <8% (per ASTM E8).
- Inert Environment Control:
- Oxygen content <0.1% (99.999% Ar/N₂), suppressing oxidation (oxide inclusion <0.02 vol%);
- Substrate preheating (200-400°C for Ti/alloys) minimizes thermal gradients (<10³ K/mm).
- Layer Precision:
- Powder layer thickness 20-50 μm, Z-axis positioning accuracy ±5 μm (linear motor drive), achieving Ra 5-15 μm surface roughness.
Quantified Advantages of SLM
| Metric | SLM | SLS | EBM |
|---|---|---|---|
| Density | >99.5% | 60-85% | 95-98% |
| Tensile Strength | Near wrought (±5%) | 60-70% of cast | 90-95% of wrought |
| Dimensional Accuracy | ±0.05-0.1 mm | ±0.2-0.5 mm | ±0.1-0.3 mm |
| Post-Processing | None required | HIP + machining | Surface polishing |
Industrial Applications of SLM
- Topology-Optimized Structures: Aerospace fuel nozzles (40% weight reduction, 22% flow efficiency gain);
- Gradient Materials: Ti-Ta orthopedic implants (elastic modulus gradient 3-110 GPa);
- Microchannel Heat Exchangers: 3D IC cooling systems (50 μm channel resolution, 300% thermal conductivity improvement).

3. Electron Beam Melting (EBM)
Similar to laser selective sintering and laser selective melting processes, electron beam selective melting technology (EBSM) is a rapid manufacturing technology that uses high-energy and high-speed electron beams to selectively bombard metal powders, thereby melting and forming powder materials.
The Process of EBSM Technology
First, spread a layer of powder on the powder-laying plane;
Then, the electron beam selectively melts according to the information of the cross-sectional profile under the control of a computer. The metal powder is melted together under the bombardment of the electron beam and bonded to the formed part below, stacked layer by layer until the entire part is completely melted;
Finally, remove the excess powder to obtain the required three-dimensional product.
The real-time scanning signal of the host computer is transmitted to the deflection coil after digital-to-analog conversion and power amplification. The electron beam is deflected under the magnetic field generated by the corresponding deflection voltage to achieve selective melting. After more than ten years of research, it was found that orthogonal experiments were conducted on some process parameters such as electron beam current, focusing current, action time, powder thickness, acceleration voltage, and scanning method. The action time has the greatest impact on molding.
Advantages and Disadvantages of Electron Beam Melting (EBM)
| Advantages | Disadvantages |
|---|---|
| Complete melting of powder leads to high density and strength. | Small print volume (maximum diameter 350 mm, height 380 mm). |
| High strength due to high density compared to other metal 3D printing technologies. | Slightly lower accuracy due to the laser spotlight being wider. |
| Faster printing process. | Limited material selection (only titanium or chrome-cobalt alloy). |
| Non-sintered powders can be recycled. | Expensive machine and materials ($300+/kg). |
| Lower risk of warping due to vacuum. |

4. Laser Melting Molding Technology (LMD)
Laser Metal Deposition (LMD), first developed by Sandia National Laboratories in 1995, is a subset of Directed Energy Deposition (DED). Globally, it is also termed Laser Cladding Forming (LCF), Direct Energy Deposition (DED), or Laser Engineered Net Shaping (LENS™). Despite regional nomenclature differences, its core mechanism relies on spatiotemporal coupling between a high-energy laser beam (1064-1070 nm wavelength) and coaxial/off-axis powder feeding systems.
Laser cladding is a complex physical and chemical metallurgical process. The parameters in the cladding process have a great influence on the quality of the cladding parts. The process parameters in laser cladding mainly include laser power, spot diameter, defocus, powder feeding speed, scanning speed, molten pool temperature, etc. They have a great influence on the dilution rate, cracks, surface roughness and density of the cladding layer. At the same time, the various parameters also affect each other, which is a very complex process. Appropriate control methods must be used to control various influencing factors within the range allowed by the cladding process.
Process Dynamics and Multiphysics Coupling
LMD builds layered structures through:
- Coaxial nozzle delivery of metallic powder (45-150 μm, 0.5-20 g/min) with carrier gas (Ar/He);
- Laser beam (500-4000 W, 0.5-3 mm spot) focusing to create transient melt pools (1600-3000°C peak, 10-500 ms duration);
- 3D motion systems (±5 μm precision) driving melt pool trajectories at 0.2-2 m/s, achieving metallurgical bonding with layer thicknesses of 50-200 μm.
Parameter Interactions and Defect Formation
- Energy Density Window: Laser power density (10^4-10^6 W/cm²) and powder flux must align to stabilize melt pools. Deviations cause porosity (>3%) or unmelted particles.
- Dilution Control: Substrate melting depth (50-300 μm) must be limited to 5-15% to prevent composition segregation (e.g., Fe diffusion in Inconel 718/304L systems causing γ’ phase coarsening).
- Thermal Stress Management: Rapid cooling (10^3-10^5 K/s) induces residual stress (>500 MPa), mitigated via interlayer temperature control (200-400°C) or preheating (300-800°C).
Cutting-Edge Optimization Strategies
| Challenge | Solution | Outcome |
|---|---|---|
| High Parameter Sensitivity | Machine learning real-time tuning (Bayesian optimization + digital twins) | 80% faster process window identification |
| Anisotropy | Ultrasonic impact treatment (UIT) for dislocation rearrangement | 300% fatigue life improvement |
| Geometric Complexity Limits | 5-axis motion + adaptive slicing algorithms | 30° overhang angles (support-free) |

5. Metal Filament Extrusion (FFF & FDM)
Metal Filament Extrusion (MFE) integrates the framework of FDM/FFF processes with powder metallurgy principles. Its core workflow includes: filament blending (55–65 vol% metal powder + polymer binder) → low-temperature deposition (180–220°C) → debinding and sintering (1300–1600°C). Currently at the industrialization threshold, its techno-economic characteristics are summarized below:
Table 1. Techno-Economic Balance Matrix of Metal Filament Extrusion
| Dimension | Advantages | Challenges |
|---|---|---|
| Process Environment | Ambient conditions (25°C, 1 atm) | Long debinding/sintering cycles (48–72 hrs) with ±0.5% dimensional tolerance control required. |
| Equipment Cost | Hardware costs 1/10 of SLM technology (approx. 5k–5k–20k) | Post-processing relies on high-temperature furnaces (50k–50k–200k), raising total ownership costs. |
| Material Compatibility | Supports multi-material switching (316L stainless steel, titanium alloys, tungsten). | High polymer content leads to post-sintering porosity >15% (density <90% theoretical). |
| Mechanical Properties | Tensile strength of sintered parts: 200–400 MPa (suitable for non-load-bearing prototypes). | Significant anisotropy (Z-axis strength = 60–70% of X/Y-axis). |
| Precision Control | Deposition layer resolution: 50 μm (comparable to plastic FDM). | Sintering shrinkage rate of 15–20% requires geometric compensation algorithms. |
Breakthrough Directions
| Bottleneck | Innovative Solutions | Target Parameters |
|---|---|---|
| Low sintered density | Nano-binder formulations + pressure-assisted sintering (10–50 MPa). | Density ≥95% theoretical, porosity <5%. |
| Poor dimensional stability | AI-driven shrinkage compensation (CT scan feedback-based). | Net dimensional tolerance ±0.1 mm (ASTM F3187). |
| Multi-material interface defects | Gradient filament co-extrusion (layer-wise composition gradation). | Interfacial shear strength ≥80% of matrix strength. |
Application Positioning:
Rapid prototyping: Deliver metal-look functional prototypes within 48 hrs (cost = 1/5 of traditional machining).
Educational tools: Safe, low-cost platforms for metal AM training.
Artistic design: Direct fabrication of intricate hollow structures in precious metals (silver, copper).

Baosheng Industry Commonly Used Metal 3D Printing Materials
The list of metal type options in metal 3D printing materials is long and growing. However, the most commonly used metal types are:
Stainless steel: Generally divided into 3 alloys: 304, 316 and 17-4. These alloys are corrosion resistant and have high strength when non-porous.
Tool steels D2, A2 and H13: High strength, hardenable, wear resistant, suitable for molds and tools.
Titanium and Ti64: High strength materials suitable for lightweight parts.
Aluminum 7075, 4047, 6061, 2319, 4043: These are various lightweight alloys used for general purpose lightweight parts.
Inconel® 718, 625: These materials have low corrosion and high temperature resistance and are suitable for uses such as engine parts.
Cobalt chromium: Super alloys used in biomedical and aerospace applications.
Gold/silver: Pure metals used in jewelry and limited biomedical uses.
Niobium, niobium zirconium: These are high temperature resistant, highly chemical corrosion resistant alloys used in aerospace.
Tantalum: Similar to niobium, but with better chemical resistance.
Hastelloy® Nickel-Chromium: Tough material – resistant to high temperatures and cracking. Often used in turbines and nuclear components.
Tungsten and alloys: Ultra-high density materials. Often used in radiation shielding, collimators and engine components.
How Baosheng Can Help
Baosheng provides a wide range of manufacturing capabilities, including CNC machining, Sheet Metal Fabrication, 3D Printing and other services for all of your prototyping and production needs. Get started on your injection molding services or CNC machining quote with us today.